Technical Specifications Sustarin® C ESD 90 - ASTM

Test MethodUnitGuideline Value
DensitéASTM D792g / cm31.33
Water Absorption 24 hoursASTM D570%1.0
Dissipation FactorASTM D1501MHz0.005
Water Absorption SaturationASTM D570%2.0
Test MethodUnitGuideline Value
HardnessASTM D2240Shore D86
Tensile Strength at yield 73°FASTM D638psi11000
Tensile ModulusASTM D638psi425000
Elongation at BreakASTM D638%30
Flexural StrengthASTM D790psi18000
Flexural ModulusASTM D790psi450000
Compressive StrengthASTM D695psi8,000
Rockwell HardnessASTM D78586
Rockwell HardnessASTM D785R120
Shear StrengthASTM D732psi6,000
Izod Impact, NotchedASTM D256ft-lb/in1.0-1.8
Coefficient of Friction, Dynamic0.2
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.7
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-54.8
Melting Point°F330
Continuous Service Temperature, Air°F180
Deflection Temperature at 1.8Mpa (264psi)ASTM D648°F250
Flammability, UL941/8 inchHB
Test MethodUnitGuideline Value
Dielectric constantASTM D1501MHz3.7
Dielectric strengthASTM D149V/mil400
Surface resistivityASTM D257Ω/cm109-10^11
Test MethodUnitGuideline Value
FDANo
NSFNo
USDANo

Contact

Vous avez la possibilité de joindre des fichiers à votre message. Les fichiers doivent être des documents JPEG, PNG, BMP, PDF. Veuillez vous assurer que vous ajoutez uniquement des fichiers de moins de 8 Mo

Information on data protection can be found here.

renouveler
 
Search

Refine Results

Contact

Share

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
Plastiques pour applications techniques

Industrial