Test MethodUnitGuideline Value
DensitéASTM D792g / cm31.41
Water AbsorptionASTM D570%0.9
Water Absorption 24 hoursASTM D570%0.2
Test MethodUnitGuideline Value
HardnessASTM D2240Shore D85
Tensile Strength at yield 73°FASTM D638psi9500
Tensile ModulusASTM D638psi400000
Elongation at BreakASTM D638%40
Flexural StrengthASTM D790psi12000
Flexural ModulusASTM D790psi400000
Rockwell HardnessASTM D78588
Rockwell HardnessASTM D785R120
Izod Impact, NotchedASTM D256ft-lb/in1.2
Coefficient of Friction, Dynamic0.21
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.6
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-55.5
Melting Point°F330
Continuous Service Temperature, Air°F180
Deflection Temperature at 1.8Mpa (264psi)ASTM D648°F225
Deflection Temperature at 1.8Mpa (66psi)ASTM D648°F320
Flammability, UL941/8 inchHB
Test MethodUnitGuideline Value
Surface resistivityASTM D257Ω/cm1016
Test MethodUnitGuideline Value
FDAYes

Contact

Vous avez la possibilité de joindre des fichiers à votre message. Les fichiers doivent être des documents JPEG, PNG, BMP, PDF. Veuillez vous assurer que vous ajoutez uniquement des fichiers de moins de 8 Mo

Information on data protection can be found here.

renouveler
 
Search

Refine Results

Contact

Share

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
Plastiques pour applications techniques

Industrial