Technical Specifications Sustarin® C ESD 90 - ASTM

Test MethodUnitGuideline Value
DensityASTM D792g / cm31.33
Water Absorption 24 hoursASTM D570%1.0
Dissipation FactorASTM D1501MHz0.005
Water Absorption SaturationASTM D570%2.0
Test MethodUnitGuideline Value
HardnessASTM D2240Shore D86
Tensile Strength at yield 73°FASTM D638psi11000
Tensile ModulusASTM D638psi425000
Elongation at BreakASTM D638%30
Flexural StrengthASTM D790psi18000
Flexural ModulusASTM D790psi450000
Compressive StrengthASTM D695psi8,000
Rockwell HardnessASTM D78586
Rockwell HardnessASTM D785R120
Shear StrengthASTM D732psi6,000
Izod Impact, NotchedASTM D256ft-lb/in1.0-1.8
Coefficient of Friction, Dynamic0.2
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.7
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-54.8
Melting Point°F330
Continuous Service Temperature, Air°F180
Deflection Temperature at 1.8Mpa (264psi)ASTM D648°F250
Flammability, UL941/8 inchHB
Test MethodUnitGuideline Value
Dielectric constantASTM D1501MHz3.7
Dielectric strengthASTM D149V/mil400
Surface resistivityASTM D257Ω/cm109-10^11
Test MethodUnitGuideline Value
FDANo
NSFNo
USDANo

Contact

메시지에 파일을 첨부할 수 있습니다. 파일은 JPEG, PNG, BMP, PDF 문서여야 합니다. 파일 크기가 8MB 이하인지 확인하세요.

Information on data protection can be found here.

Renew
 
Search

Refine Results

Contact

Share

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
기술 응용 분야를 위한 플라스틱

Industrial