Sustarin® C MG - ASTM

POM-C

QR-Code

Characteristics

  • High mechanical strength
  • High stiffness
  • Good impact strength
  • Multi-sterilisable with hot steam, plasma as well as ethylene oxide
  • Low moisture absorption

Industries

Technical Specifications Sustarin® C MG - ASTM

Test MethodUnitGuideline Value
DensityASTM D792g / cm31.41
Water AbsorptionASTM D570%0.9
Water Absorption 24 hoursASTM D570%0.2
Test MethodUnitGuideline Value
HardnessASTM D2240Shore D85
Tensile Strength at yield 73°FASTM D638psi9500
Tensile ModulusASTM D638psi400000
Elongation at BreakASTM D638%40
Flexural StrengthASTM D790psi12000
Flexural ModulusASTM D790psi400000
Rockwell HardnessASTM D78588
Rockwell HardnessASTM D785R120
Izod Impact, NotchedASTM D256ft-lb/in1.2
Coefficient of Friction, Dynamic0.21
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.6
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-55.5
Melting Point°F330
Continuous Service Temperature, Air°F180
Deflection Temperature at 1.8Mpa (264psi)ASTM D648°F225
Deflection Temperature at 1.8Mpa (66psi)ASTM D648°F320
Flammability, UL941/8 inchHB
Test MethodUnitGuideline Value
Surface resistivityASTM D257Ω/cm1016
Test MethodUnitGuideline Value
FDAYes

Contact

메시지에 파일을 첨부할 수 있습니다. 파일은 JPEG, PNG, BMP, PDF 문서여야 합니다. 파일 크기가 8MB 이하인지 확인하세요.

Information on data protection can be found here.

Renew
 
Search

Refine Results

Contact

Share

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
기술 응용 분야를 위한 플라스틱

Industrial