DuroProtect® (and LignoProtect®) are specially developed ballistic materials. The different specifications are designed to protect against:
Combinations of these special characteristics are possible. DuroProtect® and LignoProtect® are certified, inter alia, in accordance to UL 752, EN 1522/1523, VPAM PM2007.
SKU | Name | Type | Type | Color | Measurements | Length | Width | Thickness | Height | ||
---|---|---|---|---|---|---|---|---|---|---|---|
No stock item (MOQ) | 336452 | DuroProtect® 1000 pressed | sheet | sheet | 2.445 x 1.255 x 12 (+/-0,635) mm | 2,445 mm | 1,255 mm | 12 mm | |||
No stock item (MOQ) | 348807 | DuroProtect® 1000 pressed | sheet | sheet | 2.440 x 1.220 x 8,1 mm | 2,440 mm | 1,220 mm | 8.1 mm | |||
No stock item (MOQ) | 348808 | DuroProtect® 1000 pressed | sheet | sheet | 2.440 x 1.220 x 6,35 (-0,13/+1,78) mm | 2,440 mm | 1,220 mm | 6.35 mm | |||
No stock item (MOQ) | 429884 | DuroProtect® 1000 pressed | sheet | sheet | 2.440 x 1.220 x 6,2 mm | 2,440 mm | 1,220 mm | 6.2 mm | |||
No stock item (MOQ) | 461134 | DuroProtect® 1000 pressed | sheet | sheet | 2.440 x 1.220 x 12 (+/-0,635) mm | 2,440 mm | 1,220 mm | 12 mm | |||
No stock item (MOQ) | 471010 | DuroProtect® 1000 pressed | sheet | sheet | 2.445 x 1.255 x 6,2 (+/-0,35) mm | 2,445 mm | 1,255 mm | 6.2 mm |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Part Number | 1717 | ||
Standard Color | Off-White |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Compressive Strength | ASTM D 695 | psi | 70,000 |
IZOD Impact Strength (notched) | ASTM D 256 | ft. lb./in. | 52 |
Tensile Strength, lengthwise | ASTM D 638 | psi | 45,000 |
Tensile Strength, crosswise | ASTM D 638 | psi | 40,000 |
Flexural Strength, lengthwise | ASTM D 790 | psi | 16,800 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
UL Recognition File Number | BP10588 | ||
Coefficient of Thermal Expansion | ASTM D 696 | (in./in.°C) x 10-5 | 2.0 |
Thermal Conductivity | ASTM C 177 | 2.0 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Level 2 | ASTM E 119 | Passed | |
Level 1 | UL 94 | HB | |
Level 2 and above | UL 94 | V0 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Density | ASTM D 792 | lbs/ft3 | 125 |
Water Absorption | ASTM D 570 | % by wt. | 1.4 |
Barcol Hardness | ASTM D 2583 | 50 |