Test MethodUnitGuideline Value
DensityASTM D792g / cm31.15
Water AbsorptionASTM D570%8.5
Water Absorption 24 hoursASTM D570%1.0
Dissipation FactorASTM D1501MHz0.02
Test MethodUnitGuideline Value
Tensile Strength at YieldASTM D638psi12000
HardnessASTM D2240Shore D85
Tensile ModulusASTM D638psi450000
Tensile ElongationASTM D638%25
Flexural StrengthASTM D790psi17000
Flexural ModulusASTM D790psi460000
Compressive StrengthASTM D695psi16000
Rockwell HardnessASTM D78585
Rockwell HardnessASTM D785R115
Shear StrengthASTM D732psi10500
Izod Impact, NotchedASTM D256ft-lb/in0.6
Coefficient of Friction, Dynamic0.23
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.7
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-54.0
Melting PointASTM D789°F495
Continuous Service Temperature, Air°F220
Flammability, UL941/8 inchHB
Deflection Temperature at 264psiASTM D648°F195
Deflection Temperature at 66psiASTM D648°F470
Test MethodUnitGuideline Value
Dielectric constantASTM D1501MHz3.8
Dielectric strengthASTM D149V/mil350
Surface resistivityASTM D257Ω/cm>1013
Test MethodUnitGuideline Value
FDANo
NSFNo
USDANo

Contact

You have the option of attaching files to your message. The files have to be JPEG, PNG, BMP, PDF-documents. Please be sure that you only add files up to 8 MB

Information on data protection can be found here.

Obnovit
 
Search

Refine Results

Kontakt

Share

Přihlášení k odběru newsletteru

Select Website

Roechling_Industrial_Banner.jpg
Plasty pro technické použití

Industrial