Glastherm® HT 220 is suitable for processes with a continuous operating temperature of up to 220 °C (428 °F) and combines a high level of heat insulation with a very high compressive strength in high temperatures. Glastherm® HT 220 is free of asbestos and can be easily cut and adapted with standard metal tools.
SKU | Name | Type | Type | Color | Measurements | Length | Width | Thickness | Height | ||
---|---|---|---|---|---|---|---|---|---|---|---|
No stock item (MOQ) | 270973 | Glastherm® HT 220 pressed | sheet | sheet | 2.440 x 1.220 x 32 (+/-1,5) mm | 2,440 mm | 1,220 mm | 32 mm | |||
No stock item (MOQ) | 285590 | Glastherm® HT 220 pressed | sheet | sheet | 2.440 x 1.220 x 22 (+/-1,4) mm | 2,440 mm | 1,220 mm | 22 mm | |||
No stock item (MOQ) | 288785 | Glastherm® HT 220 pressed | sheet | sheet | 2.440 x 1.220 x 9 (+/-0,7) mm | 2,440 mm | 1,220 mm | 9 mm | |||
No stock item (MOQ) | 288786 | Glastherm® HT 220 pressed | sheet | sheet | 2.440 x 1.220 x 11 (+/-0,9) mm | 2,440 mm | 1,220 mm | 11 mm | |||
No stock item (MOQ) | 299833 | Glastherm® HT 220 pressed | sheet | sheet | 1.900 x 1.000 x 11 (+/-0,9) mm | 1,900 mm | 1,000 mm | 11 mm | |||
No stock item (MOQ) | 341384 | Glastherm® HT 220 pressed | sheet | sheet | 2.440 x 1.220 x 43 (+/-1,65) mm | 2,440 mm | 1,220 mm | 43 mm | |||
No stock item (MOQ) | 353042 | Glastherm® HT 220 pressed | sheet | sheet | 1.900 x 1.000 x 73 (+/-2,2) mm | 1,900 mm | 1,000 mm | 73 mm | |||
Stock item (no MOQ) | 415641 | Glastherm® HT 220 pressed | sheet | sheet | 2.440 x 1.220 x 20 (+/-1,4) mm | 2,440 mm | 1,220 mm | 20 mm | |||
Stock item (no MOQ) | 415643 | Glastherm® HT 220 pressed | sheet | sheet | 2.440 x 1.220 x 25 (+/-1,45) mm | 2,440 mm | 1,220 mm | 25 mm | |||
Stock item (no MOQ) | 441358 | Glastherm® HT 220 pressed | sheet | sheet | 1.900 x 1.000 x 20 (+/-1,3) mm | 1,900 mm | 1,000 mm | 20 mm | |||
Stock item (no MOQ) | 449068 | Glastherm® HT 220 pressed | sheet | sheet | 1.900 x 1.000 x 22 (+/-1,4) mm | 1,900 mm | 1,000 mm | 22 mm |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Density | ISO 1183 | g / cm3 | 1,85 |
Flexural strength ┴ | ISO 178 | MPa | 360 |
Modulus of elasticity in flexion ┴ | ISO 178 | MPa | 18000 |
Compressive strength 1)┴ | ISO 604 | MPa | 500 |
Compressive strength 1)┴ +200°C | ISO 604 | MPa | 360 |
Tensile strength II | ISO 527 | MPa | 280 |
Impact strength ┴ (Charpy) | ISO 179 | kJ / m2 | 150 |
Splitting force II | DIN 53463 | N | 4000 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Thermal conductivity 2)┴ | W / (m * K) | ≈ 0,25 | |
Coefficient of linear expansion II | TMA (Mettler) | 10-6 x K-1 | ≈ 10 - 15 |
Max. continuous operating temperature | °C | 220 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Water absorption (4mm thickness) | ISO 62 | % | 0,1 |