SKU | Name | Type | Type | Color | Measurements | Length | Width | Thickness | Height | ||
---|---|---|---|---|---|---|---|---|---|---|---|
No stock item (MOQ) | 606670 | Sustarin® C brown extruded | sheet | sheet | mahogany brown, similar RAL 8016 | 50 x 620 x 1000 mm | 1,000 mm | 620 mm | 50 mm | ||
No stock item (MOQ) | 720976 | Sustarin® C brown extruded | rod | rod | mahogany brown, similar RAL 8016 | Ø 90 x 3000 mm | 3,000 mm | 90 mm | |||
No stock item (MOQ) | 720978 | Sustarin® C brown extruded | rod | rod | mahogany brown, similar RAL 8016 | Ø 90 x 1000 mm | 1,000 mm | 90 mm | |||
No stock item (MOQ) | 800844 | Sustarin® C brown extruded | rod | rod | chestnut brown, similar RAL 8015 | Ø 20 x 3000 mm | 3,000 mm | 20 mm | |||
No stock item (MOQ) | 800877 | Sustarin® C brown extruded | rod | rod | chestnut brown, similar RAL 8015 | Ø 12 x 3000 mm | 3,000 mm | 12 mm | |||
No stock item (MOQ) | 801052 | Sustarin® C brown extruded | rod | rod | chestnut brown, similar RAL 8015 | Ø 15 x 3000 mm | 3,000 mm | 15 mm | |||
No stock item (MOQ) | 921652 | Sustarin® C brown extruded | sheet | sheet | fawn brown, similar RAL 8007 | 40 x 620 x 3000 mm | 3,000 mm | 620 mm | 40 mm | ||
No stock item (MOQ) | 931949 | Sustarin® C brown extruded | rod | rod | chestnut brown, similar RAL 8015 | Ø 20 x 1000 mm | 1,000 mm | 20 mm | |||
No stock item (MOQ) | 934782 | Sustarin® C brown extruded | sheet | sheet | mahogany brown, similar RAL 8016 | 80 x 620 x 2000 mm | 2,000 mm | 620 mm | 80 mm | ||
No stock item (MOQ) | 934784 | Sustarin® C brown extruded | sheet | sheet | mahogany brown, similar RAL 8016 | 50 x 620 x 2000 mm | 2,000 mm | 620 mm | 50 mm |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Density | DIN EN ISO 1183-1 | g / cm3 | 1,41 |
Water absorption | DIN EN ISO 62 | % | 0,2 |
Flammability (Thickness 3 mm / 6 mm) | UL 94 | HB / HB |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Yield stress | DIN EN ISO 527 | MPa | 67 |
Elongation at break | DIN EN ISO 527 | % | 30 |
Tensile modulus of elasticity | DIN EN ISO 527 | MPa | 2800 |
Notched impact strength | DIN EN ISO 179 | kJ / m2 | 6 |
Shore hardness | DIN EN ISO 868 | scale D | 81 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Melting temperature | ISO 11357-3 | °C | 165 |
Thermal conductivity | DIN 52612-1 | W / (m * K) | 0,31 |
Thermal capacity | DIN 52612 | kJ / (kg * K) | 1,50 |
Coefficient of linear thermal expansion | DIN 53752 | 10-6 / K | 110 |
Service temperature, long term | Average | °C | -50 … 100 |
Service temperature, short term (max.) | Average | °C | 140 |
Heat deflection temperature | DIN EN ISO 75, Verf. A, HDT | °C | 110 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Dielectric constant | IEC 60250 | 3,8 | |
Dielectric dissipation factor (50 Hz) | IEC 60250 | 0,002 | |
Volume resistivity | DIN EN 62631-3-1 | Ω * cm | 1013 |
Surface resistivity | DIN EN 62631-3-2 | Ω | 1013 |
Comparative tracking index | IEC 60112 | 600 | |
Dielectric strength | IEC 60243 | kV / mm | 40 |