Test Method | Unit | Guideline Value | |
---|---|---|---|
Density | DIN EN ISO 1183-1 | g / cm3 | 1,45 |
Water absorption | DIN EN ISO 62 | % | ≤0,20 |
Flammability (Thickness 0,9 mm … 3 mm) | DIN 4102 | B1 | |
Flammability (Thickness 0,9 mm … 3 mm) | NF P 92-501 | M1 | |
Flammability (Thickness 1,2 mm) | BS 476 Part 7 | Class 1 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Yield stress | DIN EN ISO 527 | MPa | 55 |
Elongation at break | DIN EN ISO 527 | % | 15 |
Tensile modulus of elasticity | DIN EN ISO 527 | MPa | 3000 |
Notched impact strength | DIN EN ISO 179 | kJ / m2 | 4 |
Shore hardness | DIN EN ISO 868 | scale D | 83 |
Ball indentation hardness | DIN EN ISO 2039-1 | MPa | 110 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Thermal conductivity | DIN 52612-1 | W / (m * K) | 0,16 |
Vicat softening temperature | DIN EN ISO 306, Vicat B | °C | 76 |
Service Temperature | °C | -15 ... +60 | |
Coefficient of linear thermal expansion | DIN EN ISO 11359-2 | mm/m K | ∼ 0,075 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Dielectric constant | IEC 60250 | 3,2 | |
Dielectric dissipation factor (106 Hz) | IEC 60250 | 0,02 | |
Volume resistivity | DIN EN 62631-3-1 | Ω * cm | >1015 |
Surface resistivity | DIN EN 62631-3-2 | Ω | >1013 |