Test Method | Unit | Guideline Value | |
---|---|---|---|
Densité | DIN EN ISO 1183-1 | g / cm3 | >0,94 |
Water absorption | DIN EN ISO 62 | % | 0,01 |
Flammability (Thickness 3 mm / 6 mm) | UL 94 | HB |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Yield stress | DIN EN ISO 527 | MPa | >19 |
Tensile modulus of elasticity | DIN EN ISO 527 | MPa | >700 |
Shore hardness | DIN EN ISO 868 | scale D | >60 |
Compressive strength | ISO 3597-3 | N/mm² | 3 - 6 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Melting temperature | ISO 11357-3 | °C | 130 ... 135 |
Thermal conductivity | DIN 52612-1 | W / (m * K) | 0,41 |
Thermal capacity | DIN 52612 | kJ / (kg * K) | 1,90 |
Service temperature, long term | Average | °C | -20 … 80 |