Technical Specifications Sustamid® 66 MO - ASTM

Test MethodUnitGuideline Value
DensityASTM D792g / cm31.15
Water AbsorptionASTM D570%8.5
Water Absorption 24 hoursASTM D570%1.0
Dissipation FactorASTM D1501MHz0.02
Test MethodUnitGuideline Value
Tensile Strength at YieldASTM D638psi12000
HardnessASTM D2240Shore D85
Tensile ModulusASTM D638psi450000
Tensile ElongationASTM D638%25
Flexural StrengthASTM D790psi17000
Flexural ModulusASTM D790psi460000
Compressive StrengthASTM D695psi16000
Rockwell HardnessASTM D78585
Rockwell HardnessASTM D785R115
Shear StrengthASTM D732psi10500
Izod Impact, NotchedASTM D256ft-lb/in0.6
Coefficient of Friction, Dynamic0.23
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2 /°F1.7
Coefficient of Linear Thermal ExpansionASTM D696in/in/°F x10-54.0
Melting PointASTM D789°F495
Continuous Service Temperature, Air°F220
Flammability, UL941/8 inchHB
Deflection Temperature at 264psiASTM D648°F195
Deflection Temperature at 66psiASTM D648°F470
Test MethodUnitGuideline Value
Dielectric constantASTM D1501MHz3.8
Dielectric strengthASTM D149V/mil350
Surface resistivityASTM D257Ω/cm>1013
Test MethodUnitGuideline Value
FDANo
NSFNo
USDANo

Contact

메시지에 파일을 첨부할 수 있습니다. 파일은 JPEG, PNG, BMP, PDF 문서여야 합니다. 파일 크기가 8MB 이하인지 확인하세요.

Information on data protection can be found here.

Renew
 
Search

Refine Results

Contact

Share

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
기술 응용 분야를 위한 플라스틱

Industrial