US

Please select a language / region

 

Sustarin® H (Delrin® ) AF 20 - ASTM

POM-H

QR-Code

Characteristics

  • Good dimensional stability
  • Good wear properties
  • Good sliding properties

Technical Specifications Sustarin® H (Delrin® ) AF 20 - ASTM

Test MethodUnitGuideline Value
Specific GravityASTM D792g / cm31.54
Water Absorption 24 hoursASTM D570%0.2
Dissipation FactorASTM D1501MHz0.009
Water Absorption SaturationASTM D570%0.8
Test MethodUnitGuideline Value
HardnessASTM D785Shore DD76
Tensile Strength at yield 73°FASTM D638psi6630
Tensile ModulusASTM D638psi540000
Elongation at BreakASTM D638%30
Flexural StrengthASTM D790psi12500
Flexural ModulusASTM D790psi405000
Compressive StrengthASTM D695psi12600
Rockwell HardnessASTM D785M50
Rockwell HardnessASTM D785RR110
Test MethodUnitGuideline Value
Thermal Conductivityin/hr/ft2/F°2
CTE, linearASTM D696in/in/°F4.4x10-5
Melting PointASTM D3418°F350
Deflection Temperature at 1.8Mpa (264psi)ASTM D648°F244
Deflection Temperature at 1.8Mpa (66psi)ASTM D648°F334
Continuous Use°F185
Flammability, UL941/8 inchHB
Test MethodUnitGuideline Value
Dielectric constantASTM D1503.1
Dielectric strengthASTM D149V/mil400
Surface resistivityASTM D257Ω/cm1016
Test MethodUnitGuideline Value
FDANo
NSFNo
USDANo

Contact

You have the option of attaching files to your message. The files have to be JPEG, PNG, BMP, PDF-documents. Please be sure that you only add files up to 8 MB

Information on data protection can be found here.

Renew
 
Search

Refine Results

Contact

Share

Newsletter Registration

Select Website

Roechling_Industrial_Banner.jpg
Plastics for technical Applications

Industrial