Test Method | Unit | Guideline Value | |
---|---|---|---|
Density | ASTM D792 | g / cm3 | 0.94 |
Water Absorption | ASTM D570 | % | 0.01 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Wear resistance | Sand-slurry | 100 | |
Hardness | ASTM D2240 | Shore D | 62 - 66 |
Tensile Strength at yield 73°F | ASTM D638 | psi | 3000 |
Tensile Modulus | ASTM D638 | psi | 100000 |
Elongation at Break | ASTM D638 | % | >290 |
Flexural Strength | ASTM D790 | psi | 3200 |
Compressive Strength | ASTM D695 | psi | 2900 |
Coefficient of Friction, Dynamic | 0.10-0.22 | ||
Coefficient of Friction, Static | 0.15-0.20 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
CTE, linear | ASTM D696 | in/in/°F | 1.1 x 10-4 |
Melting Point | °F | 266 - 275 | |
Maximum Service Temperature, Air | °F | 180 | |
Heat Deflection Temperature 264psi | ASTM D648 | °F | 108 |
Flammability, UL94 | 1/8 inch | HB |
Test Method | Unit | Guideline Value | |
---|---|---|---|
Dielectric constant | ASTM D150 | 1MHz | 2.3 |
Surface resistivity | ASTM D257 | Ω/sq | 106 - 1011 |
Test Method | Unit | Guideline Value | |
---|---|---|---|
FDA | Yes | ||
NSF | No | ||
USDA | No |